Hello

Is it possible to distinguish the valence state of an ion, say manganese,
in different compounds of the same structure (say LiMn2O4 from
Li0.3Mn2O4, both Fd3m) using x-ray powderdiffractometry? Can it be done
or is it not possible to measure this difference?

Thanks for all comments...