Re: Sepiolite structure wanted.....

Alan Hewat, ILL Grenoble ( (no email) )
Mon, 30 Mar 1998 12:30:10 +0200

>I`m so interested in sepiolite structure.... I`d like to know if this
>structure has been resolved and/or published.

>From ICSD-for-WWW, Mg8 (O H)4 Si12 O30 (Sepiolite )
Brauner K, Preisinger A
Tschermaks Mineralogische und Petrographische 6 (1956) P. 120-140
Longchambon H
Bulletin de la Societe Francaise de Mineralogie 60 (1937) P. 232-276

Alan Hewat, ILL Grenoble, FRANCE <hewat@ill.fr> tel (33) 4.76.20.72.13
ftp://ftp.ill.fr/pub/dif fax (33) 4.76.48.39.06 http://www.ill.fr/dif/