Re: Si standard

Enver Akdogan ( eka@rci.rutgers.edu )
Wed, 15 Jul 1998 11:32:13 -0400 (EDT)

Jaap:

You may want to get in touch with D. Smith in State College, PA.

Cheers,

Koray

E.K. AKDOGAN
CENTER FOR CERAMIC RESEARCH
RUTGERS UNIVERSITY
PISCATAWAY, NJ 08855-0909
PHONE: (908)-445-5567
FAX: (908)-445-3258
E-MAIL: eka@rci.rutgers.edu

On Wed, 15 Jul 1998, Jaap Vente wrote:

>
> Dear all,
>
> I am after some silicon to use as an internal standard for high
> temperature x-ray diffraction. Sadly enough, NIST has run out of their
> standard 640b. Does anyone know an alternative supplier of silicon of a
> similar grade, or even better is someone happy to sell a bit of their
> stock.
>
> Regards
>
> Jaap Vente
>
>
>
> Dr. Ir. J.F. Vente
> Inorganic Chemistry Laboratory
> Department of Chemistry
> University of Oxford
> South Parks Road
> Oxford, OX1 3QR
> United Kingdom
> E-mail: jaap.vente@chem.ox.ac.uk
> tel: (..44)(0)1865-272602
> Fax: (..44)(0)1865-272690
>
>