Re: using FULLPROF to refine PSD data

R. Young ( (no email) )
Mon, 07 Sep 1998 10:44:45 -0400

Dear Tao:

Please do not refine the data.

At 03:08 AM 9/6/1998 -0700, you wrote:
>Dear All,
>
>I am thinking using FULLPROF to do refinement with some data collected on
>an Inel diffractometer with an incident beam momochromator and a curved
>position sensitive detector (PSD). GSAS doesn't work well with these data,

Jim Elliott has an Inel curved PSD and is now getting excellent results
with it. He is doing Rietveld refinements with DBWS or GSAS or, probably,
both. His group did spend a lot of time calibrating the PSD and otherwise
getting to the point where they are getting these good results.

He has been in the States for some weeks and is scheduled to be back in
London either this week or next. His e-mail address is

j.c.elliott@mds.qmw.ac.uk

Sincerely,
R. A. Young