Hi,
I found a file named INST_XRY.PRM in \gsas\example. This file contains the following lines.

++++++++++++++++++++
123456789012345678901234567890123456789012345678901234567890
INS BANK 1
INS DTYPE STND
INS HTYPE PXCR
INS 1 IRAD 3
INS 1 ICONS 1.540500 1.544300 0.0 0 0.5 0
INS 1I HEAD DUMMY INCIDENT SPECTRUM FOR X-RAY DIFFRACTOMETER
INS 1I ITYP 0 0.0000 180.0000 1
INS 1PRCF1 2 6 0.01
INS 1PRCF11 2.000000E+00 -2.000000E+00 5.000000E+00 0.000000E+00
INS 1PRCF12 0.000000E+00 0.000000E+00
++++++++++++++++++++

Please tell me the meanings of everyline. So I can modify this file according to the parameters in my machine.