>Dear Rietvelders,
>
> Could somebody recommend the most suitable Rietveld software,
>freeware (GSAS, DBWS ??), that can handle at least 8 phases and a
>LARGE absorption contrast, elements at least 2 to 3 periods apart.
> I have been using SIROQUANT, but it seems to have a limitation on
>the magnitude of the differnce in absorption contrast.
> Any information would be very much appreciated.
>
>Sincerely,
>Quirina
>
> \|||/
> (o o)
>*----oOO------(_)-OOo---------*
>
> Quirina I. Roode
> PhD student: Cement Chemistry
>*-----------------------------*
>Department of Civil Engineering
>University of the Witwatersrand
> P O Wits, 2050, Johannesburg
> SOUTH AFRICA
>*-----------------------------*Oooo.
> ROODE@civen.civil.wits.ac.za ( )
> Tel: +27-(0)11-716-2478 (w) ) /
> Fax: +27-(0)11-339-1762 (w) (_/
>*.oooO------------------------*
> ( )
> \ (
> \_)
>
Linda D. Mansker Chemical and Nuclear Engineering
209 Farris Engr. Bldg. University of New Mexico
Page: (505) 251-5970 Albuquerque, NM 87131-1341
FAX: (505) 277-5433 EMAIL:mansker@unm.edu
--------------------------------------------------------------------
"The most beautiful experience we can have is the mysterious. ...
the fundamental emotion which stands at the cradle of true art
and true science." Albert Einstein, 'Living Philosophies'
---------------------------------------------------------------------