absorption contrast?

Quirina Roode ( (no email) )
Mon, 27 Apr 1998 10:10:05 GMT+2

Dear Rietvelders,

Could somebody recommend the most suitable Rietveld software,
freeware (GSAS, DBWS ??), that can handle at least 8 phases and a
LARGE absorption contrast, elements at least 2 to 3 periods apart.
I have been using SIROQUANT, but it seems to have a limitation on
the magnitude of the differnce in absorption contrast.
Any information would be very much appreciated.

Sincerely,
Quirina

\|||/
(o o)
*----oOO------(_)-OOo---------*

Quirina I. Roode
PhD student: Cement Chemistry
*-----------------------------*
Department of Civil Engineering
University of the Witwatersrand
P O Wits, 2050, Johannesburg
SOUTH AFRICA
*-----------------------------*Oooo.
ROODE@civen.civil.wits.ac.za ( )
Tel: +27-(0)11-716-2478 (w) ) /
Fax: +27-(0)11-339-1762 (w) (_/
*.oooO------------------------*
( )
\ (
\_)