Paolo G. Radaelli wrote:

... [many useful comments deleted]
>
> By the way: maybe you know this, but GSAS does not have default values for
> the magnetic form factors, so youo have to input them by hand and, oddly
> enough, save them with the option "U" in the form factor menu.
>

Dear Paolo,

Right! I was bit by this at first. After I found the correspondence
between the coefficients in the Int'l Tables and the GSAS names, I must
have typed them in 3 or 4 times before realizing I needed to update the
file with the "U" option before leaving that screen.

Your message has cleared up much of my confusion. Thanks for your help.

--John Henry